Maki 310/310S bakin karfe 8.0 * 0.3mm nannade tubing / capillary tubing
Kemikal Haɗin Kan Bakin Karfe 310/310S
A sinadaran abun da ke ciki na sa 310 da sa 310S bakin karfe an taƙaita a cikin wadannan tebur.
Maki 310/310S bakin karfe 8.0 * 0.3mm nannade tubing / capillary tubing
Tebur 1.Chemical abun da ke ciki% na sa 310 da 310S bakin karfe
Haɗin Sinadari | 310 | 310S |
Carbon | 0.25 max | 0.08 max |
Manganese | 2.00 max | 2.00 max |
Siliki | 1.50 max | 1.50 max |
Phosphorus | 0.045 max | 0.045 max |
Sulfur | 0.030 max | 0.030 max |
Chromium | 24.00 - 26.00 | 24.00 - 26.00 |
Nickel | 19.00 - 22.00 | 19.00 - 22.00 |
Kayayyakin Injini na Daraja 310/310S Bakin Karfe
The inji Properties na sa 310 da sa 310S bakin karfe an taƙaita a cikin wadannan tebur.
Maki 310/310S bakin karfe 8.0 * 0.3mm nannade tubing / capillary tubing
Table 2.Kaddarorin injina na sa 310/310S bakin karfe
Kayayyakin Injini | 310/310S |
Mataki 0.2 % Tabbacin Damuwa MPa (minti) | 205 |
Ƙarfin Tensile MPa (minti) | 520 |
Tsawaita % (min) | 40 |
Hardness (HV) (max) | 225 |
Abubuwan Jiki na Bakin Karfe na Ferritic
An taƙaita kaddarorin jikin mutum na sa 310 da sa 310S bakin karfe a cikin tebur mai zuwa.
Maki 310/310S bakin karfe 8.0 * 0.3mm nannade tubing / capillary tubing
Table 3.Kaddarorin jiki na sa 310/310S bakin karfe
Kayayyaki | at | Daraja | Naúrar |
Yawan yawa |
| 8,000 | kg/m3 |
Wutar Lantarki | 25°C | 1.25 | %IACS |
Juriya na Lantarki | 25°C | 0.78 | Micro ohm.m |
Modulus na Elasticity | 20°C | 200 | GPA |
Modulus Shear | 20°C | 77 | GPA |
Rabon Poisson | 20°C | 0.30 |
|
Narkar da Rnage |
| 1400-1450 | °C |
Takamaiman Zafi |
| 500 | J/kg.°C |
Dangantakar Magnetic Permeability |
| 1.02 |
|
Thermal Conductivity | 100°C | 14.2 | W/m.°C |
Adadin Faɗawa | 0-100°C | 15.9 | /°C |
0-315 ° C | 16.2 | /°C | |
0-540°C | 17.0 | /°C |