KARFE KARFE NA SIHE na zamani ne a fasahar kere-kere kamar yadda ka'idojin kasa da kasa da sabbin sabbin abubuwa suka yi.Muna ba da fifiko mai yawa akan Marufi da lakabi don Samar da samfuran Ingantattun samfuran ga Abokin Ciniki da na Ƙasashen waje.Hastelloy C276 kayan aiki an cika su a hankali tare da yadudduka na foils na filastik da Bubble nannade kuma a hankali sanya su cikin Akwatunan katako.
Da fatan za a kira mu don ƙarin zurfafa duban ƙarin amfani waɗanda suka haɗa da wasu kwatancen bayanan juriya na lalata, kafofin watsa labarai, ƙima da yanayin zafi.Don ƙarin bayani kan SIHE STEEL's Pipe da Tsarin Bututu, da fatan za a duba bututunmu na Hastelloy C276 da Hastelloy C276 Tube shafukan.
Hastelloy C276 | Ni | C | Mo | Mn | Si | Fe | P | S | Co | Cr |
| Ma'auni | 0.010 max | 15.00 - 17.00 | 1.00 max | 0.08 max | 4.00 - 7.00 | 0.04 max | 0.03 max | 2.5 max | 14.50 - 16.50 |
Hastelloy C276 Kayayyakin Injini
Hannun Hannun Yanayin Wuta na Daki na Abubuwan da aka Rushe
Samfurin Samfura | Tensile (ksi) | .2% Haihuwa (ksi) | Tsawaita % |
Alloy C276 Bar | 110.0 | 52.6 | 62 |
Alloy C276 Plate | 107.4 | 50.3 | 67 |
Alloy C276 Takardar bayanai | 115.5 | 54.6 | 60 |
Alloy C276 Tube & Alloy C276 Bututu | 105.4 | 45.4 | 70 |
Hastelloy C276 Meting Point
Abubuwan Jiki | °F | Raka'a ta Burtaniya | °C | Ma'auni Raka'a |
Yawan yawa | 72 | 0.321 lb./in.(3) | 22 | 8.89g/cm(3) |
Rage Narkewa | 2415- | 1323- | ||
Lantarki | 75 | 51 microhm-in. | 24 | 1.30 microhm-m |
Ma'ana Coefficient | 75-200 | 6.2 microin./in.-°F | 24-93 | 11.2 X 10(-6)m/mK |
75-400 | 6.7 microin./in.-°F | 24-204 | 12.0 X 10(-6)m/mK | |
75-600 | 7.1 microin./in.-°F | 24-316 | 12.8 X 10(-6)m/mK | |
75-800 | 7.3 microin./in.-°F | 24-427 | 13.2 X 10(-6)m/mK | |
75-1000 | 7.4 microin./in.-°F | 24-538 | 13.4 X 10(-6)m/mK | |
75-1200 | 7.8 microin./in.-°F | 24-649 | 14.1 X 10(-6)m/mK | |
75-1400 | 8.3 microin./in.-°F | 24-760 | 14.9 X 10(-6)m/mK | |
75-1600 | 8.8 microin./in.-°F | 24-871 | 15.9 X 10(-6)m/mK | |
75-1700 | 8.9 microin./in.-°F | 24-927 | 16.0 X 10(-6)m/mK | |
Thermal | -270 | 50 Btu-in/ft²-hr-°F | -168 | 7.2 W/mK |
-100 | 60 Btu-in/ft²-hr-°F | -73 | 8.6 W/mK | |
0 | 65 Btu-in/ft²-hr-°F | 32 | 9.4 W/mK | |
100 | 71 Btu-in/ft²-hr-°F | 38 | 10.2 W/mK | |
200 | 77 Btu-in/ft²-hr-°F | 93 | 11.1 W/mK | |
400 | 90 Btu-in/ft²-hr-°F | 204 | 13.0 W/mK | |
600 | 104 Btu-in/ft²-hr-°F | 316 | 15.0 W/mK | |
800 | 117 Btu-in/ft²-hr-°F | 427 | 16.9 W/mK | |
1000 | 132 Btu-in/ft²-hr-°F | 538 | 19.0 W/mK | |
1200 | 145 Btu-in/ft²-hr-°F | 649 | 20.9 W/mK | |
1400 | 159 Btu-in/ft²-hr-°F | 760 | 22.9 W/mK | |
1600 | 173 Btu-in/ft²-hr-°F | 871 | 24.9 W/mK | |
1800 | 185 Btu-in/ft²-hr-°F | 982 | 26.7 W/mK | |
2000 | 195 Btu-in/ft²-hr-°F | 1093 | 28.1 W/mK |
Hastelloy C276 Daidai
STANDARD | UNS | Ayyukan Aiki NR. | AFNOR | EN | JIS | BS | GOST |
Hastelloy C276 | N10276 | 2.4819 | - | NiMo16Cr15W | Farashin 0276 | - | ХН65МВУ |
Ƙayyadaddun samfur
ASTM B622, B829 / ASME SB622, SB829 / NACE MR0175
Girman Rage
Wajen Diamita (OD) | Kaurin bango |
.250-500" | .035-065" |
An gama sanyi da bututu mai haske.
Abubuwan Bukatun Sinadarai
Alloy C276 (UNS N10276)
Abun ciki %
Ni Nickel | Cr Chromium | Mo Molybdenum | Fe Iron | W Tungsten | C Carbon | Si Siliki | Co Cobalt | Mn Manganese | V Vanadium | P Phosphorous | S Sulfur |
57.0 min | 14.5-16.5 | 15.0-17.0 | 4.0-7.0 | 3.0-4.5 | 0.010 max | 0.08 max | 2.5 max | 1.0 max | 0.35 max | 0.04 max | 0.03 max |
Hakuri Mai Girma
OD | Haƙuri OD | Haƙurin bango |
.250-500" | +.004”/-.005” | ± 15% |
Kayayyakin Injini
Ƙarfin Haɓaka: | 41 ku min |
Ƙarfin Ƙarfafawa: | 100 ksi min |
Tsawaitawa (minti 2): | 40% |